看E版的测试boye钴金表现比我预想的差很多   这个测试我估计6K和TALONITE代表的非钢会集体获胜
hound 发表于 2009-7-6 09:13 
很难说。
虽然从已有的信息看6k和talonite应该获胜,而且应该是完胜,但是看了boye钴的较差表现我心里还是打鼓的。毕竟如果6k和talonite不是以至少3~4倍的优势完胜的话,那和厂家,刀匠宣传的就相差甚远了。而boye钴,竟然连30V都未胜!{:3_66:}
boye钴是boye自造的产物,从他公布的信息看成分很像stellite 6B,但是很难说他做的钴晶能达到那两个大厂的标准。
另外boye钴表现不佳的原因很可能和它的低硬度有关,我这两天确定了一下,boye的硬度只有接近40(非常接近stellite 6B的硬度,38)。厂家标称stellite 6K的硬度是47,talonite的硬度是49左右。
boye女儿给我的回信截文:
You had asked about the toughness of the cobalt Basic 3.  For many years we made the 
Basic 3 in both dendritic stainless (440C) and dendritic cobalt.  People would often ask 
us about the differences.
440C Dendritic stainless is Rc 57-58.  Dendritic cobalt is Rc 40.  The steel is harder, 
but the cobalt cuts faster and holds an edge longer (and it doesn't rust).  David (the 
knifemaker) prefers cobalt as his everyday carry. |
|